Grades | Stainless Steels | X2CrTi17

AFNOR X2CrTi17 ( Ferrite )

PDF | Word | Print

X2CrTi17 Application:Stainless steels - Part 3: Technical delivery conditions for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes

Chemical composition(mass fraction)(wt.%) of the X2CrTi17
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.025
Si - 0.50
Mn - 0.50
P - 0.040
S - 0.015
Cr 16.00 18.00
Mo - -
Ni - -
Ti 0.30 0.60
N - 0.015

Mechanical properties of grade X2CrTi17

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
998 (≥) 431 (≥) 32 33 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 212

Physical properties of grade X2CrTi17

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
543 (≥) 136 (≥) 23 11 14 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
591 746 848 - - -

X2CrTi17 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED