Grades | Stainless Steels | Z11CN17-08

AFNOR Z11CN17-08

PDF | Word | Print

Z11CN17-08 Application:Stainless steels for general purposes. Plates, wide strips and strips

Chemical composition(mass fraction)(wt.%) of the Z11CN17-08
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.09 0.12
Si - 0.75
Mn 0.75 1.20
P - 0.040
S - 0.015
Cr 16.50 17.50
Mo - -
Ni 7.00 8.00

Mechanical properties of grade Z11CN17-08

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
854 (≥) 166 (≥) 41 14 11 Solution and Aging, Annealing, Ausaging, Q+T,etc 243

Physical properties of grade Z11CN17-08

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
924 (≥) 253 (≥) 33 24 42 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
859 675 182 - - -

Z11CN17-08 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED