Z15CN16-02 Application:Rolling stock. Recommanded steels for rolling stock construction. IX: stainless steels for general purposes

Chemical composition(mass fraction)(wt.%) of the Z15CN16-02
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.15 0.20
Si - 1.00
Mn - 1.00
P - 0.040
S - 0.025
Cr 15.50 17.00
Mo - -
Ni 1.50 2.50

Mechanical properties of grade Z15CN16-02

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
687 (≥) 815 (≥) 21 12 44 Solution and Aging, Annealing, Ausaging, Q+T,etc 424

Physical properties of grade Z15CN16-02

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
937 (≥) 568 (≥) 43 14 43 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
886 444 852 - - -

Z15CN16-02 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED