Grades | Stainless Steels | 20CrMnVTiB4-10

AFNOR 20CrMnVTiB4-10

PDF | Word | Print

20CrMnVTiB4-10 Application:Steels and nickel alloys for fasteners with specified elevated and/or low temperature properties

Chemical composition(mass fraction)(wt.%) of the 20CrMnVTiB4-10
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.17 0.23
Si - 0.40
Mn 0.35 0.75
P - 0.020
S - 0.020
Cr 0.90 1.20
Ni - 0.20
Mo 0.90 1.10
Ti 0.07 1.50
V 0.60 0.80
Al 0.015 0.080
As - 0.20
B 0.001 0.010
Cu - 0.20
Sn - 0.20

Mechanical properties of grade 20CrMnVTiB4-10

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
235 (≥) 559 (≥) 22 32 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 323

Physical properties of grade 20CrMnVTiB4-10

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
678 (≥) 839 (≥) 42 11 44 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
477 855 148 - - -

20CrMnVTiB4-10 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED