Grades | Stainless Steels | Ni-Mo28

AFNOR Ni-Mo28

PDF | Word | Print

Ni-Mo28 Application:Nickel and nickel alloys. Nickel-molybdenum and nickel-molybdenum- chromium-alloys

Chemical composition(mass fraction)(wt.%) of the Ni-Mo28
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.05
Si - 1.00
Mn - 1.00
P - 0.025
S - 0.030
Cr - 1.00
Ni - remaining
Mo 26.00 30.00
V 0.20 0.40
Co - 2.50

Mechanical properties of grade Ni-Mo28

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
756 (≥) 896 (≥) 44 13 32 Solution and Aging, Annealing, Ausaging, Q+T,etc 413

Physical properties of grade Ni-Mo28

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
168 (≥) 128 (≥) 13 11 12 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
913 147 768 - - -

Ni-Mo28 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED