Grades | Stainless Steels | 09X14H16Б

GOST 09X14H16Б ( Austenite )

PDF | Word | Print

09X14H16Б Application:Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(mass fraction)(wt.%) of the 09X14H16Б
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.07 0.12
Si - 0.60
Mn 1.00 2.00
P - 0.035
S - 0.020
Cr 13.00 15.00
Ni 14.00 17.00
Mo - 0.30
W - 0.20
Ti - 0.20
Nb 0.90 1.30

Mechanical properties of grade 09X14H16Б

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
836 (≥) 291 (≥) 21 32 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 241

Physical properties of grade 09X14H16Б

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
115 (≥) 276 (≥) 44 43 32 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
164 472 255 - - -

09X14H16Б Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED