Grades | Stainless Steels | X45Cr13

DIN X45Cr13 ( Austenite )

PDF | Word | Print

X45Cr13 Application:Corrosion-resistant high-temperature steel

Chemical composition(mass fraction)(wt.%) of the X45Cr13
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.35 0.44
Si - 0.6
Mn - 0.6
Ni - 0.6
S - 0.025
P - 0.03
Cr 12 14

Mechanical properties of grade X45Cr13

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
382 (≥) 635 (≥) 12 12 41 Solution and Aging, Annealing, Ausaging, Q+T,etc 322

Physical properties of grade X45Cr13

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
115 (≥) 939 (≥) 31 43 11 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
722 549 386 - - -

X45Cr13 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED