Grades | Stainless Steels | 08X18H12Б

GOST 08X18H12Б ( Austenite )

PDF | Word | Print

08X18H12Б Application:Russia GOCT standard stainless steel and heat resistant steel steel grade and chemical composition

Chemical composition(mass fraction)(wt.%) of the 08X18H12Б
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si - 0.80
Mn - 2.00
P - 0.035
S - 0.020
Cr 17.00 19.00
Ni 11.00 13.00
Mo - 0.30
W - 0.20
Ti 5×C 0.70
Nb 10×C 1.10

Mechanical properties of grade 08X18H12Б

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
123 (≥) 397 (≥) 42 31 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 221

Physical properties of grade 08X18H12Б

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
344 (≥) 543 (≥) 32 32 13 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
375 925 352 - - -

08X18H12Б Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED