Grades | Stainless Steels | XH33TMДЮ(ЭK63,BHC-45)

GOST XH33TMДЮ(ЭK63,BHC-45)

PDF | Word | Print

XH33TMДЮ(ЭK63,BHC-45) Application:Russia TY standard corrosion resistant alloy hot rolled and forged bars

Chemical composition(mass fraction)(wt.%) of the XH33TMДЮ(ЭK63,BHC-45)
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.01 0.05
Si - 0.40
Mn 1.00 1.50
S 0.15 0.25
P 0.06 0.12
Cr 13.00 15.00
Ni 32.00 35.00
Mo 1.50 2.00
Ti 2.50 3.00
Al 0.70 1.00
Cu 1.00 1.50
Ca - 0.05

Mechanical properties of grade XH33TMДЮ(ЭK63,BHC-45)

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
284 (≥) 778 (≥) 44 12 14 Solution and Aging, Annealing, Ausaging, Q+T,etc 122

Physical properties of grade XH33TMДЮ(ЭK63,BHC-45)

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
422 (≥) 338 (≥) 43 24 32 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
566 745 366 - - -

XH33TMДЮ(ЭK63,BHC-45) Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED