Grades | Stainless Steels | STR616

KS STR616 ( Martensite )

PDF | Word | Print

STR616 Application:Heat - resisting steel bars

Chemical composition(mass fraction)(wt.%) of the STR616
Elements Min.(≥) Max.(≤) Similar Remarks
C 0.20 0.25
Si - 0.50
Mn 0.50 1.00
P - 0.04
S - 0.03
Cr 11.00 13.00
Ni 0.50 1.00
Mo 0.75 1.25
N - -
Cu - 0.30
W 0.75 1.25
V 0.20 0.30

Mechanical properties of grade STR616

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
969 (≥) 387 (≥) 44 21 42 Solution and Aging, Annealing, Ausaging, Q+T,etc 423

Physical properties of grade STR616

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
844 (≥) 522 (≥) 43 14 34 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
475 991 313 - - -

STR616 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED