1.3964 Application:Non-magnetizable austenitic cast steel —G-X2CrNiMnMoNNb 21-16-5-3 Part 4: Castings

Chemical composition(mass fraction)(wt.%) of the 1.3964
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.030
Si - 1.00
Mn 4.00 6.00
P - 0.025
S - 0.010
Cr 20.00 21.50
Ni 15.00 17.00
Mo 3.00 3.50
Nb - 0.25
N 0.200 0.35

Mechanical properties of grade 1.3964

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
697 (≥) 246 (≥) 22 31 23 Solution and Aging, Annealing, Ausaging, Q+T,etc 322

Physical properties of grade 1.3964

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
259 (≥) 963 (≥) 24 31 42 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
495 111 881 - - -

1.3964 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED