Grades | Stainless Steels | ER 308

International ER 308 ( Austenite )

PDF | Word | Print

ER 308 Application:Bare Stainless Steel Welding Electrodes and Rods

Chemical composition(mass fraction)(wt.%) of the ER 308
Elements Min.(≥) Max.(≤) Similar Remarks
C - 0.08
Si 0.25 0.60
Mn 1.00 2.50
P - 0.03
S - 0.03
Cr 19.5 22.0
Ni 9.00 11.0
Cu - 0.75
Mo - 0.75

Mechanical properties of grade ER 308

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
424 (≥) 239 (≥) 41 22 33 Solution and Aging, Annealing, Ausaging, Q+T,etc 313

Physical properties of grade ER 308

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
236 (≥) 117 (≥) 44 44 24 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
594 716 976 - - -

ER 308 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED