D2(Cr12Mo1V1) Hot Rolled Plate

Hardness

  • Bar, wire, sheet; Annealed < 255 HB
  • Bar, wire, sheet; Cold drawn < 269 HB
  • Bar, wire, sheet; Heat treated > 59 HRC

Chemical Composition [%]

C 1.4000 1.6000 -
Si 0.1000 0.6000 -
Mn 0.1000 0.6000 -
P - 0.0300 -
S - 0.0300 -
Cr 11.000 13.000 -
Mo 0.7000 1.2000 -
V 0.5000 1.1000 -
Ni+Cu - 0.7500 


Heat Treatment

Preheat to 815 +/- 4℃, austenitize at either 996 +/- 12℃ in a salt bath or 1010 +/- 12℃ in a controlled atmosphere furnace for 10 to 20 minutes.
Quench in air then temper at 200℃ for 2 hours.
 

Cross Reference Table

 

D2(Cr12Mo1V1) Hot Rolled Plate Range of products
Product type Products Dimension Processes
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded

Enquiry