SS ASP 60 PM

Location » Home » Grades > Special Alloy > ASP 60 PM

Grades | Special Alloy | ASP 60 PM

SS ASP 60 PM

Print

ASP 60 PM Application:Carbide for cutting tools

Chemical composition(mass fraction)(wt.%) of the ASP 60 PM
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Mo(%) V(%) W(%) Co(%)
2.25-2.40 ≤0.45 ≤0.40 ≤0.030 ≤0.030 3.70-4.50 6.50-7.30 6.00-6.70 6.00-6.80 9.80-11.0

Mechanical properties of grade ASP 60 PM

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
889 (≥) 557 (≥) 34 42 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 434

Physical properties of grade ASP 60 PM

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
856 (≥) 593 (≥) 23 22 33 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
238 419 573 - - -

ASP 60 PM Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED