40X15H7Γ7Φ2

Location » Home » Grades > Special Alloy > 40X15H7Γ7Φ2

Grades | Special Alloy | 40X15H7Γ7Φ2

40X15H7Γ7Φ2

Print

40X15H7Γ7Φ2 Application:Austenitic

Chemical composition(mass fraction)(wt.%) of the 40X15H7Γ7Φ2
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) V(%) W(%) Ti(%)
0.38-0.47 0.90-1.40 6.00-8.00 Max 0.035 Max 0.02 14.0-16.0 6.00-8.00 0.65-0.95 1.50-1.90 Max 0.20 Max 0.20

Mechanical properties of grade 40X15H7Γ7Φ2

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
674 (≥) 979 (≥) 12 34 31 Solution and Aging, Annealing, Ausaging, Q+T,etc 341

Physical properties of grade 40X15H7Γ7Φ2

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
948 (≥) 437 (≥) 21 12 31 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
271 981 177 - - -

40X15H7Γ7Φ2 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED