CNS Ferrite 21

Location » Home » Grades > Special Alloy > Ferrite 21

Grades | Special Alloy | Ferrite 21

CNS Ferrite 21

Print

Ferrite 21 Application:China Taiwan Heat-Resistant Steel

Chemical composition(mass fraction)(wt.%) of the Ferrite 21
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Al(%)
Max 0.10 Max 1.50 Max 1.00 0.04 0.03 17.0-21.0 0.60 2.00-4.00

Mechanical properties of grade Ferrite 21

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
739 (≥) 796 (≥) 43 14 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 312

Physical properties of grade Ferrite 21

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
424 (≥) 188 (≥) 32 44 12 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
995 392 116 - - -

Ferrite 21 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED