GBT GH2136

Location » Home » Grades > Special Alloy > GH2136

Grades | Special Alloy | GH2136

GBT GH2136

Print

GH2136 Application:Age hardening type iron base alloy

Chemical composition(mass fraction)(wt.%) of the GH2136
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) Al(%) Ti(%) Other(%)
≤0.06 0.75 0.35 0.025 0.025 13.0-16.0 24.5-28.5 1.00-1.75 ≤0.35 2.40-3.20 B:0.005-0.025,V00.1-0.10

Mechanical properties of grade GH2136

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
381 (≥) 774 (≥) 13 43 13 Solution and Aging, Annealing, Ausaging, Q+T,etc 341

Physical properties of grade GH2136

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
979 (≥) 966 (≥) 31 32 34 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
731 166 364 - - -

GH2136 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED