Grades | Stainless Steels | X1NiCrMoCu31-27-4, 1.4563, Alloy 28, UNS N08028
AFNOR X1NiCrMoCu31-27-4, 1.4563, Alloy 28, UNS N08028 ( Austenite )
PDF | Word | Print
X1NiCrMoCu31-27-4, 1.4563, Alloy 28, UNS N08028 Application:Seamless circular steel tubes for mechanical and general engineering purposes - Technical delivery conditions - Austenitic steel designed to deal with sour gas, phosphoric, sulphuric and acetic acids, and vinyl chloride. It is used for heat exchangers, co
| Elements | Min.(≥) | Max.(≤) | Similar | Remarks |
|---|---|---|---|---|
| C | - | 0.020 | ||
| Si | - | 0.70 | ||
| Mn | - | 2.00 | ||
| P | - | 0.030 | ||
| S | - | 0.010 | ||
| Cr | 26.00 | 28.00 | ||
| Mo | 3.00 | 4.00 | ||
| Ni | 30.00 | 32.00 | ||
| N | - | 0.11 | ||
| Cu | 0.70 | 1.50 |
| Yield Rp0.2 (MPa) |
Tensile Rm (MPa) |
Impact KV (J) |
Elongation A (%) |
Reduction in cross section on fracture Z (%) |
As-Heat-Treated Condition | HBW |
|---|---|---|---|---|---|---|
| 659 (≥) | 437 (≥) | 13 | 41 | 12 | Solution and Aging, Annealing, Ausaging, Q+T,etc | 433 |
| Property | Density kg/dm3 |
Temperature T °C/F |
Specific heat J / kgK |
Thermal conductivity W/mK |
Electric resistance µΩ·cm |
|---|---|---|---|---|---|
| 326 (≥) | 689 (≥) | 21 | 12 | 43 | Solution and Aging, Annealing, Ausaging, Q+T,etc |
| Temp. °C/°F |
Creep strain limit (10000h) (Rp1,0) N/mm2 |
Creep rupture strength (10000h) (Rp1,0) N/mm2 |
- | - | - |
| 236 | 784 | 789 | - | - | - |
| Product type | Products | Dimension | Processes | Deliver Status |
|---|---|---|---|---|
| Plates / Sheets | Plates / Sheets | 0.08-200mm(T)*W*L | Forging, hot rolling and cold rolling | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
| Steel Bar | Round Bar, Flat Bar, Square Bar | Φ8-1200mm*L | Forging, hot rolling and cold rolling, Cast | Black, Rough Turning, Shot Blasting, |
| Coil / Strip | Steel Coil /Steel Strip | 0.03-16.0x1200mm | Cold-Rolled & Hot-Rolled | Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting |
| Pipes / Tubes | Seamless Pipes/Tubes, Welded Pipes/Tubes | OD:6-219mm x WT:0.5-20.0mm | Hot extrusion, Cold Drawn, Welded | Annealed, Solution and Aging, Q+T, ACID-WASHED |