ГОСТ 09X16H15M3Б

Print

09X16H15M3Б Application:Austenitic

Chemical composition(mass fraction)(wt.%) of the 09X16H15M3Б
C(%) Si(%) Mn(%) P(%) S(%) Cr(%) Ni(%) Mo(%) W(%) Nb(%) Ti(%)
Max 0.09 Max 0.80 Max 0.80 Max 0.035 Max 0.02 15.0-17.0 14.0-16.0 2.50-3.00 Max 0.20 0.60-0.90 Max 0.20

Mechanical properties of grade 09X16H15M3Б

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
693 (≥) 492 (≥) 23 24 43 Solution and Aging, Annealing, Ausaging, Q+T,etc 132

Physical properties of grade 09X16H15M3Б

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
894 (≥) 162 (≥) 42 23 12 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
679 916 178 - - -

09X16H15M3Б Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED