Grades | Tool Die Steels | T3

SAE T3

PDF | Word | Print

T3 Application:High-Speed Tool Steel

Chemical composition(mass fraction)(wt.%) of the T3
Elements Min.(≥) Max.(≤) Similar Remarks
C 1.08 1.13
Si 0.20 0.40
Mn 0.10 0.40
Cr 4.00 4.25
Mo 0.70 0.90
V 2.90 3.30
W 18.00 18.50

Mechanical properties of grade T3

Yield
Rp0.2 (MPa)
Tensile
Rm (MPa)
Impact
KV (J)
Elongation
A (%)
Reduction in cross section on fracture
Z (%)
As-Heat-Treated Condition HBW
832 (≥) 515 (≥) 33 32 24 Solution and Aging, Annealing, Ausaging, Q+T,etc 313

Physical properties of grade T3

Property Density
kg/dm3
Temperature T
°C/F
Specific heat
J / kgK
Thermal conductivity
W/mK
Electric resistance
µΩ·cm
891 (≥) 731 (≥) 24 21 14 Solution and Aging, Annealing, Ausaging, Q+T,etc
Temp.
°C/°F
Creep strain limit
(10000h)
(Rp1,0) N/mm2
Creep rupture strength
(10000h)
(Rp1,0) N/mm2
- - -
827 659 648 - - -

T3 Range of products
Product type Products Dimension Processes Deliver Status
Plates / Sheets Plates / Sheets 0.08-200mm(T)*W*L Forging, hot rolling and cold rolling Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Steel Bar Round Bar, Flat Bar, Square Bar Φ8-1200mm*L Forging, hot rolling and cold rolling, Cast Black, Rough Turning, Shot Blasting,
Coil / Strip Steel Coil /Steel Strip 0.03-16.0x1200mm Cold-Rolled & Hot-Rolled Annealed, Solution and Aging, Q+T, ACID-WASHED, Shot Blasting
Pipes / Tubes Seamless Pipes/Tubes, Welded Pipes/Tubes OD:6-219mm x WT:0.5-20.0mm Hot extrusion, Cold Drawn, Welded Annealed, Solution and Aging, Q+T, ACID-WASHED